on saturday i got some OOP rhino ram things (real world name Cullin device)
i only manage to get two, one the comb shaped one and one with three spikeon. my first task was to single piece mold the comb one
long story short, i got three made, but the mold is now a bit warped, so i will re-heat it and make s few of the three pronged ones.
but here is the top tip-
IF you get hold of an old, OOP bit that you want to cast lots of in future, FOR FUCKS SAKE dont make three or four then use the original. Keep your "masters" in a separate box never to be used. you cant make a mold of a copy, they are too soft. so keep the originals safe!!